The method for oxygenation of fused grain-oriented ceramics on the basis of YBa2Cu3O7-? (??-YBCO) in isostatic pressures includes its heating, conditioning to oxygenation of fused grain-oriented ceramics and its cooling. The method is performed in a gasostat. Pre-heating is made to temperature of beginning ortho-tetra transition of the structure YBa2Cu3O7-? (Y123) in inert gas flow at atmospheric pressure. It is continued ceramics heating. Step-by-step, inert gas is substituted for oxygen so that after the temperature lower than the temperature of fusing the structure Y123 have been reached, ceramics is conditioned at atmospheric pressure over the time of that fully enough for substitution inert gas for oxygen. Next cooling is performed in two stages. At the first stage, ceramics is cooling to temperature of finishing Y123 ortho-tetra transition simultaneously pressure is increased to values, at which oxygenation in equal condition for given temperature is occurred, and then ceramics is conditioned at this temperature to its oxygenation. At the second stage the heating is removed and ceramics is cooled in gasostat to the room temperature, then pressure is removed.
机译:基于YBa2Cu3O7-α的熔融晶粒取向陶瓷的氧化方法等静压下的(β-YBCO)包括其加热,对熔融的取向陶瓷的氧合的调节和冷却。该方法在恒压器中进行。预热至结构YBa 2 Cu 3 O 7-α的开始正交转变的温度。 (Y123)在大气压下呈惰性气体流动。继续进行陶瓷加热。逐步地,用惰性气体代替氧气,以便在达到低于融合结构Y123的温度的温度之后,在大气压下将陶瓷调至大气压以充分替代惰性气体。接下来的冷却分两个阶段进行。在第一阶段,将陶瓷冷却至完成的Y123正交转变的温度,同时将压力增加至一定值,在该温度下,在给定温度下会以相同的条件发生氧合,然后将陶瓷在此温度下调节至其氧合。在第二阶段,去除加热,并在恒温器中将陶瓷冷却至室温,然后去除压力。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号