PROBLEM TO BE SOLVED: To provide a molding method of a transparent thermoplastic resin for obtaining a product having good optical characteristics or a large-sized glazing product of a construction machine, a car, a bus or the like and to provide this large-sized glazing product. ;SOLUTION: A molded article reduced in optical strain is obtained by the injection compression molding of a transparent thermoplastic resin. In this case, an injection speed is set to 300 mm/sec or more and, when the glass transition temp. of the thermoplastic resin is set to Tg, a main mold is held to temp. lower than Tg and the highest temp. of a cavity surface and a core surface at a time when the thermoplastic resin is in contact with the cavity surface of a mold and the core surface is set to [Tg+1]-[Tg+50]°C.;COPYRIGHT: (C)2001,JPO
机译:解决的问题:提供一种透明热塑性树脂的成型方法,该成型方法用于获得具有良好光学特性的产品或建筑机械,汽车,公共汽车等的大型玻璃制品,并提供这种大型玻璃产品。 ;解决方案:通过注塑压缩成型透明热塑性树脂获得光学应变降低的成型品。在这种情况下,将注射速度设定为300mm / sec以上,并且当玻璃化转变温度为100mm / sec时。将热塑性树脂的温度设定为Tg,将主模具保持在温度。低于Tg和最高温度。热塑性树脂与模具的型腔表面接触并且型芯表面设置为[Tg + 1]-[Tg + 50]℃时型腔表面和型芯表面的接触角:日本特许厅(C)2001

著录项

  • 公开/公告号JP4090634B2

    专利类型

  • 公开/公告日2008-05-28

    原文格式PDF

  • 申请/专利权人 帝人化成株式会社;

    申请/专利号JP19990223950

  • 发明设计人 帆高 寿昌;

    申请日1999-08-06

  • 分类号B29C45/56;B29C45/73;B29C45/77;B29C45/78;B29K101/12;

  • 国家 JP

  • 入库时间 2022-08-21 20:18:47

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号