An improved process for the preparation of high grade synthetic retile from limonite with pig iron as a by-product, the said process comprising, subjecting limonite to reduction with 30-100% coal (w/w) at a temperature in the range of 850-1250°C for a period of 2-6 hours, cooling and removing unreacted coal to obtain a product having 80-95% metallisation; smelting the metallised ilmenite mixed with less than 10% carbon (w/w) in a transferred arc plasma using arc current in the range of 100-400 amps, are voltage of 20-60 V under flow of inert gas at a range of 0 -2 litre/minute for a fixed time in the range 1-5 minutes; separating the metal as pig iron and TiO2 as slag; grinding the slag followed by oxidation in a temperature range of 500-1000°C in the presence of an oxidizing gas for 25-30 minutes, followed by leaching the oxidized product with dilute HC1 at temperatures below 90°C for a period of 1-6 hours followed by filtration, washing and drying to obtain synthetic rutile
机译:一种从褐铁矿中以生铁为副产物制备高级合成铺面砖的改进方法,所述方法包括在850℃的温度下用30-100%的煤(w / w)还原褐铁矿。 -1250℃保持2-6小时,冷却并除去未反应的煤,得到金属化率为80-95%的产物。在100到400安培范围内的电弧电流下,在惰性气体流动范围为0的情况下,在20至60伏的电压下熔化混合了少于10%碳(w / w)的金属化钛铁矿。 -2升/分钟,固定时间为1-5分钟;分离金属为生铁和二氧化钛为炉渣;研磨炉渣,然后在氧化气体存在下于500-1000°C的温度范围内氧化25-30分钟,然后在90°C以下的温度下用稀HCl浸出氧化产物1- 6小时,然后过滤,洗涤和干燥以获得合成金红石

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号