ECO-FRIENDLY PROCESS FOR THE PRODUCTION OF SYNTHETIC RUTILE FROM ILMENITE

机译:从钛铁矿生产合成金红宝石的环保工艺

摘要

The present Invention discloses an eco-friendly process for the production of high grade synthetic rutile from llmenite and saleable Iron oxide as byproduct by leaching of the reduced ore with dilute acids. According to the present Invention the llmenite ore is beneficiated by the steps of pretreatment of the ore by oxidation in the presence of air, reduction at the temperature below 1000°C and leaching of reduced llmenite with dilute solution of ammonium chloride in aeration and consequently with sulphuric acid of lower concentration. According to this process llmenite can be beneficiated without the use of magnetic separation procedure. The high grade beneficiated llmenite achieved by the above said economic process, having significant TiOa content of 90-92% recovered from the processed mixture by suitable methods such as filtration and calcination.
机译:本发明公开了一种生态友好的方法,其通过用稀酸浸出还原的矿石由钛铁矿和可销售的副产物氧化铁生产高级合成金红石。根据本发明,通过在空气存在下进行氧化,在低于1000℃的温度下还原并在曝气中用氯化铵稀溶液浸出还原的钛铁矿的方法预处理矿石,从而对钛铁矿进行选矿。较低浓度的硫酸。根据该方法,可以在不使用磁选程序的情况下使钛铁矿受益。通过上述经济方法获得的高品位精选钛铁矿,通过合适的方法例如过滤和煅烧从加工过的混合物中回收了90-92%的明显的TiOa含量。

著录项

  • 公开/公告号IN2012CH03081A

    专利类型

  • 公开/公告日2012-08-10

    原文格式PDF

  • 申请/专利权人

    申请/专利号IN3081/CHE/2012

  • 发明设计人 DR JABEERA BASHEER;

    申请日2012-07-27

  • 分类号C22B3/00;

  • 国家 IN

  • 入库时间 2022-08-21 17:23:59