The present invention relates to a method for producing a cross-linked polyacrylamide particles by precipitation polymerization , in more detail relates to a method for producing a spherical crosslinked polyacrylamide particles having a core / shell structure with an average particle diameter of 0.1 ~ 10 in a single step using a precipitation polymerization method . In the present invention , and have the form of particles which obtain up to form a cross-linking reaction within the particles , polyacrylamide particles are provided with a self- core / shell structure during polymerization due to the reaction ratio of the difference and the difference of affinity between the solvent monomer and , polyacrylamide particles of the present invention can significantly increase the particle size can increase the degree of crosslinking compared to the conventional polymerization method can be effectively used in various industrial fields such as high-value-added information or micro device industry .
机译:沉淀聚合制备交联聚丙烯酰胺颗粒的方法本发明涉及一种通过沉淀聚合制备交联聚丙烯酰胺颗粒的方法,更详细地涉及一种制备核/壳结构平均粒径为0.1〜10的球形交联聚丙烯酰胺颗粒的方法。一步法使用沉淀聚合法。在本发明中,由于具有在粒子内达到形成交联反应的粒子的形态,因此,聚丙烯酰胺粒子在聚合过程中,由于反应比例的不同而差异,因此具有自核/壳结构。与传统的聚合方法相比,本发明的聚丙烯酰胺颗粒可以显着增加粒径,增加交联度,可以有效地用于各种工业领域,如高附加值信息或微型设备行业。

著录项

  • 公开/公告号KR100854046B1

    专利类型

  • 公开/公告日2008-08-26

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20050040322

  • 申请日2005-05-13

  • 分类号C08G73/02;C08J3/12;

  • 国家 KR

  • 入库时间 2022-08-21 19:51:43

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号