PRODUCTION METHOD OF INORGANIC FINE-PARTICLE DISPERSION SOLUTION, PRODUCTION METHOD OF ORGANIC OPTICAL ELEMENT AND TITANIUM-DIOXIDE DISPERSION LIQUID
PRODUCTION METHOD OF INORGANIC FINE-PARTICLE DISPERSION SOLUTION, PRODUCTION METHOD OF ORGANIC OPTICAL ELEMENT AND TITANIUM-DIOXIDE DISPERSION LIQUID
展开▼
机译:无机细颗粒分散液的制备方法,有机光学元素的制备方法和二氧化钛分散液
展开▼
页面导航
摘要
著录项
相似文献
摘要
PROBLEM TO BE SOLVED: To provide a production method of an inorganic fine-particle dispersion solution which suitably disperses a primary inorganic fine particle having the average particle diameter of 30 nm or below, in the degree that light scattering-permeability ability as an optical component is satisfied, and also gives the viscosity suitable for handling to the dispersion solution.;SOLUTION: In the production method of the inorganic fine-particle dispersion solution consists of dispersing a primary inorganic fine-particle having the average particle diameter of 30 nm or below in a solution, this method has a dispersion treatment step where a media having the average particle diameter of ≥15 μm and ≤30 μm is introduced into a mixed solution, in the state that the primary inorganic fine-particle having the average particle diameter of 30 nm or below is coagulated in a solvent, to be stirred to disperse the inorganic fine particle, and an ultrasonic wave is applied to the mixed solution in or just after this dispersion treatment.;COPYRIGHT: (C)2010,JPO&INPIT
展开▼
机译: (54)标题:具有硅酸盐涂层的固体颗粒(54):FESTKoRPERPARTKEL MIT SILKATBESCHICHTUNG(57)摘要:本发明涉及一种具有二氧化硅涂层的固体颗粒的生产方法,其包括以下步骤:将固体颗粒分散为将其涂覆在水性介质中以产生固体颗粒分散体,通过缓冲系统调节固体颗粒分散体的pH以产生缓冲的固体颗粒分散体,并向缓冲的固体颗粒分散体中添加碱性硅酸盐溶液以形成二氧化硅在涂覆期间将其涂覆在固体颗粒上,其中选择缓冲体系和碱性硅酸盐溶液的量,使得在添加碱性硅酸盐溶液之前和在添加完成之后,缓冲的固体颗粒分散体的pH至少为7.0。碱性硅酸盐溶液的最大含量为11.0。固体颗粒优选是无机固体,特别是