首页> 外国专利> Ni 60 mass above junction membrane and Cr which are contained 40 - 60 mass , Ni 35 mass above to consist of

Ni 60 mass above junction membrane and Cr which are contained 40 - 60 mass , Ni 35 mass above to consist of

机译:由60〜60质量%的接合膜和60%以上的Cr构成的Ni,由35质量%以上的Ni构成的由Cr构成的

摘要

PROBLEM TO BE SOLVED: To provide a water-cooling type steel-made tubular structure constituting a converter exhaust gas cooling facility, etc., wherein a film having excellent high-temperature corrosion resistance, high-temperature wear resistance, moisture condensation corrosion resistance, and film peeling resistance is formed, a facility lifetime is long, the maintenance cost and the updating cost are reduced, and the rate of operation of the facility is enhanced, and to provide a method for manufacturing the same.;SOLUTION: The water-cooling type steel-made tubular structure is constituted so that Cr alloy of 22-60 mass% effective for high-temperature wear and high-temperature corrosion is covered on a surface of the water-cooling type steel-made tubular structure, and the heating and diffusion treatment is performed for improving the peeling resistance of a film and reducing pores, and a joining layer is formed and an oxidation preventive layer is formed depending on a heating condition so that a layer of Cr alloy of 22-60 mass% is not peeled, and the method for manufacturing the same is provided.;COPYRIGHT: (C)2006,JPO&NCIPI
机译:解决的问题:提供构成转炉排气冷却设备等的水冷式钢制管状结构,其中膜具有优异的耐高温腐蚀性,耐高温磨损性,耐湿气凝结性,并且形成膜抗剥离性,延长设备寿命,降低维护成本和更新成本,并提高设备的运转率,并提供一种制造方法。构成冷却型钢制管状结构,以便在水冷型钢制管状结构的表面上覆盖对高温磨损和高温腐蚀有效的22〜60质量%的Cr合金,并进行加热。进行扩散处理以提高膜的耐剥离性和减少气孔,并根据加热条件形成接合层并形成防氧化层。提供一种不会剥落22-60质量%Cr合金层的方法,并提供其制造方法。版权所有:(C)2006,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号