β '-Al2O3 has a solid structure polycrystalline potassium ion conductor, its preparation, and the preparation of potassium metal by using a potassium ion conductor

机译:β“ -Al2O3具有固体结构的多晶钾离子导体,其制备方法以及使用钾离子导体制备金属钾的方法

摘要

PROBLEM TO BE SOLVED: To provide a solid potassium ion conductor having β"-Al2O3 structure, its manufacturing method, and a manufacturing method of potassium using the potassium ion conductor.;SOLUTION: The solid potassium ion conductor is obtained by embedding an polycrystalline alkali metal β"-Al2O3 moulding into an oxide powder containing potassium and aluminum, heating it to at least 1,100 °C at least at 100°C/Hr and, further to 1,300°C, and after maintaining for at least one hour, cooling it. The potassium metal is obtained by using potassium amalgam as a material, and by producing by electrolysis by using an anode 16 containing the potassium amalgam and a cathode 17 made of a liquid potassium metal filled inside the solid electrolyte tube 1 made of the solid potassium ion conductor, and by leading into a container 20 in an inactive atmosphere filled with paraffin, and by solidifying in a shape of a globe 23.;COPYRIGHT: (C)2006,JPO&NCIPI
机译:解决的问题:提供具有β-“-Al 2 O 3 结构的固体钾离子导体,其制造方法以及使用该钾的钾的制造方法SOLUTION:固态钾离子导体是通过将多晶碱金属β-Al 2 O 3 成型件嵌入包含钾和铝的氧化物粉末中而获得的将其加热到至少1100℃,至少以100℃/小时,然后进一步加热到1300℃,并保持至少一小时后,将其冷却。通过使用包含汞齐的材料作为阳极,并通过使用包含钾汞齐的阳极16和填充在由固体钾离子制成的固体电解质管1内部的由液态钾金属制成的阴极17的电解法来生产金属钾。导体,并在充满石蜡的惰性气氛中通入容器20中,并凝固成球形23 。;版权所有:(C)2006,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号