In this paper, wollastonite nano-powder were successfully synthesized by the surfactants modified-calcined method using calcium silicate residue of potassium feldspar after extraction of potassium and alumina. The effects of modifier and calcined temperature on the phase composition, morphology and microstructure were studied by X-ray diffraction (XRD) and scanning electron microscopy (SEM). The results showed that the phase of samples with different modifier processing is wollastonite-2M, while CTAB as modifier can avoid preferred orientation growth. The obtained wollastonite powder is spherical in morphology and well dispersed with the particle size of approximately 150nm.
机译:本文在钾和氧化铝萃取后,通过使用钾硅酸钙残留物成功地由表面活性剂改性煅烧方法成功合成了硅酸盐纳米粉。通过X射线衍射(XRD)和扫描电子显微镜(SEM)研究了改性剂和煅烧温度对相组成,形态和微观结构的影响。结果表明,具有不同改性剂处理的样品相是硅灰岩-2M,而CTAB作为改性剂可以避免优选的取向生长。所得硅灰石粉末是形态学的球形,并且良好地分散在约150nm的粒度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号