Aluminium oxide powder produced by flame hydrolysis and having a large surface area

机译:火焰水解法生产的氧化铝粉,表面积大

摘要

Aluminium oxide powder produced by flame hydrolysis and consisting of aggregates of primary particles, having a BET surface area of from 100 to 250 m2/g, a dibutyl phthalate absorption of from 50 to 450 g/100 g of aluminium oxide powder, which powder shows only crystalline primary particles in high-resolution TEM pictures. It is prepared by vaporizing aluminium chloride, transferring the vapour by means of a carrier gas to a mixing chamber and, separately therefrom, supplying hydrogen, air (primary air), which may optionally be enriched with oxygen and/or may optionally be pre-heated, to the mixing chamber, then igniting the mixture of aluminium chloride vapour, hydrogen, air in a burner and burning the flame into a reaction chamber that is separated from the surrounding air, subsequently separating the solid material from the gaseous substances and then treating the solid material with steam and optionally with air, the discharge rate of the reaction mixture from the mixing chamber into the reaction chamber being at least 10 m/s, and the lambda value being from 1 to 10 and the gamma value being from 1 to 15. It can be used as an ink-absorbing substance in ink-jet media.
机译:通过火焰水解生产的氧化铝粉末,由一次颗粒的聚集体组成,BET表面积为100至250 m 2 / g,邻苯二甲酸二丁酯吸收度为50至450 g / 100 g氧化铝粉末的示意图,该粉末在高分辨率TEM图像中仅显示晶体初级粒子。它是通过蒸发氯化铝,借助载气将蒸气传输到混合室并与之分开提供氢气,空气(一次空气)来制备的,氢气,空气(一次空气)可以可选地富含氧气和/或可以预先进行加热到混合室,然后在燃烧器中点燃氯化铝蒸气,氢气,空气的混合物,并将火焰燃烧到与周围空气分离的反应室中,随后将固体材料与气态物质分离,然后进行处理带有蒸汽和可选地带有空气的固体材料,反应混合物从混合室到反应室的排放速率至少为10 m / s,λ值为1到10,γ值为1到1。 15.它可用作喷墨介质中的吸墨物质。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号