Disclosed is a process for producing a mayenite-containing oxide that contains a mayenite-type compound and has a hydride ion density of 1 × 1018/cm3 or more, without requiring any expensive facility, control of complicated reaction conditions and a long reaction time.  Also disclosed is a process for producing an electrically conductive mayenite-containing oxide.Specifically disclosed is a process for producing a mayenite-containing oxide, which comprises the following steps: a raw material mixing step of producing a mixture comprising CaO and Al2O3 at a molar ratio of 9:10 to 14:5 in terms of oxide contents; and a hydrogenating step of calcining the mixture in a hydrogen-containing gas having a partial pressure of oxygen of 1000 Pa or less at a temperature of not lower than 1210°C and lower than 1350°C to thereby produce a mayenite-containing oxide that contains a mayenite-type compound and has a hydride ion density of 1 × 1018/cm3 or more.  Also specifically disclosed is a process for producing an electrically conductive mayenite-containing oxide that contains an electrically conductive mayenite compound, which comprises irradiating the mayenite-containing oxide with an ultraviolet ray or the like.
机译:本发明公开了一种无需任何昂贵的设备,无需复杂的反应条件,且反应时间长的,含有钙铝石型化合物,氢离子浓度为1×1018 / cm 3以上的含钙铝石的氧化物的制造方法。还公开了一种用于制备包含导电性钙铝石的氧化物的方法。具体地公开了一种制备含钙铝石的氧化物的方法,其包括以下步骤:原料混合步骤,其以氧化物含量计以9:10至14:5的摩尔比制备包含CaO和Al2O3的混合物;氢化步骤,在不低于1210℃且低于1350℃的温度下,在氧分压为1000Pa以下的含氢气体中煅烧所述混合物,从而生成含钙铝石的氧化物,所述氧化物含有钙铝石型化合物,且氢化物离子密度为1×1018 / cm3以上。还具体公开了一种用于制备包含导电性钙铝石化合物的含导电性钙铝石的氧化物的方法,该方法包括用紫外线等照射含钙铝石的氧化物。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号