The fabrication of bake hardened steel strip comprises: (a) production of a steel with a given composition; (b) casting a slab of this steel, then hot rolling to produce a strip, the end rolling temperature being greater than the Ar3 point; (c) reeling of the strip at a temperature between 500 and 700 degrees C; (d) cold rolling the strip with a reduction rate of 50 to 80 %; (e) continuous annealing heat treatment with a duration of less than 15 minutes; (f) cold drawing with a reduction rate of between 1.2 and 2.5 %. Independent claims are also included for: (i) a bake hardened steel strip produced by this method; (ii) a component able to be cut from such steel strip, then painted and heated to at least 200 degrees C.
机译:烘烤硬化钢带的制造包括:(a)生产具有给定成分的钢; (b)浇铸这种钢的板坯,然后热轧制成带材,其最终轧制温度高于Ar3点; (c)在500至700摄氏度之间的温度下卷绕带钢; (d)以50%至80%的压下率将带钢冷轧; (e)持续时间少于15分钟的连续退火热处理; (f)冷拔率在1.2%和2.5%之间。还包括以下方面的独立权利要求:(i)用这种方法生产的烘烤硬化钢带; (ii)能够从这种钢带上切割下来,然后涂漆并加热到至少200摄氏度的部件。

著录项

  • 公开/公告号DE60332951D1

    专利类型

  • 公开/公告日2010-07-22

    原文格式PDF

  • 申请/专利权人 ARCELORMITTAL FRANCE;

    申请/专利号DE20036032951T

  • 申请日2003-10-10

  • 分类号C21D8/04;C21D8/02;C21D9/52;C22C38/02;C22C38/04;C22C38/06;

  • 国家 DE

  • 入库时间 2022-08-21 18:27:01

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号