首页> 外国专利> ESTER-CROSSLINKED RUBBER AND METHOD FOR PRODUCING THE SAME, CURABLE RUBBER COMPOSITION FOR PRODUCING THE ESTER-CROSSLINKED RUBBER, AND MODIFIED COPOLYMER, AND MOLDED FORM INCLUDING THE ESTER-CROSSLINKED RUBBER

ESTER-CROSSLINKED RUBBER AND METHOD FOR PRODUCING THE SAME, CURABLE RUBBER COMPOSITION FOR PRODUCING THE ESTER-CROSSLINKED RUBBER, AND MODIFIED COPOLYMER, AND MOLDED FORM INCLUDING THE ESTER-CROSSLINKED RUBBER

机译:酯交联橡胶和生产相同,可固化的橡胶组合物的方法,所述橡胶组合物用于生产酯交联橡胶和改性的共聚物,以及包括酯交联橡胶的模制形式

摘要

PROBLEM TO BE SOLVED: To provide a highly thermally stable crosslinked rubber enabling its own production level to be made higher.;SOLUTION: The crosslinked rubber is obtained by the following process: the carbon-carbon double bonds of a rubbery copolymer obtained by copolymerizaton between 90-99.5 mol% of at least one 4-7C isomonoolefin and 0.5-10 mol% of at least one 4-14C aliphatic diene are epoxidized and/or glycolated; and the resultant copolymer is subjected to esterification reaction with a crosslinking agent having at least two functional groups capable of forming ester linkages by reaction with the resultant epoxy groups and/or hydroxy groups, to effect crosslinking. This ester-crosslinked rubber is stable even at 150°C.;COPYRIGHT: (C)2012,JPO&INPIT
机译:要解决的问题:提供一种高度热稳定的交联橡胶,以使其自身的生产水平更高。解决方案:交联橡胶是通过以下方法获得的:橡胶状共聚物的碳-碳双键是通过将90-99.5摩尔%的至少一种4-7C异单烯烃和0.5-10摩尔%的至少一种4-14C脂族二烯环氧化和/或糖基化;所得共聚物与具有至少两个能通过与所得环氧基和/或羟基反应形成酯键的官能团的交联剂进行酯化反应,以进行交联。这种酯交联的橡胶即使在150°C时也很稳定;版权所有(C)2012,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号