首页> 外国专利> Zr Ti Ni (Cu) system for the titanium low attaching it is low the fusion point low attaching filler material alloy composition

Zr Ti Ni (Cu) system for the titanium low attaching it is low the fusion point low attaching filler material alloy composition

机译:Zr Ti Ni(Cu)系统用于低附着力的钛合金低熔点低附着力的填充料合金成分

摘要

Topic Melted temperature was low, could hold down the content of the copper element, titanium low offer the filler material metal which does not decrease the durability of the assembly body which is attached.SolutionsAs for this invention, Zr Ti Ni for the titanium low attaching (Cu) system in regard to the fusion point low attaching filler material alloy composition low, Zr aTi bNi c (in formula, each, Zr, Ti and Ni atmoic % to show a, b and c, 47 a 52, 24 b 30, 22 c 26 and 0.3c/(a+c) 0.35 is shown.)So 3 original type alloy compositions of Zr Ti Ni which is displayed, or, Zr aTi bNi cCu d (in formula, a and b, each, Zr, Ti, Ni and Cu atmoic % it shows c and d, 48 a 60, 20 b 28, 19 c+d 30, 3 d 12 and 0.12d/(c+d) shows the 0.5.)So 4 original type alloy compositions of Zr Ti Ni Cu which is displayed are offered.
机译:熔融温度低,可以抑制铜元素的含量,钛低提供填充金属,而不会降低所附着的组装体的耐用性。解决方案如本发明,Zr Ti Ni用于钛关于低熔点的低附着(Cu)体系低附着填充材料合金成分低,Zr aTi bNi c (式中,Zr,Ti和Ni的原子%表示a,b和c,47 a 52,24 b 30,22 c 26和0.3 aTi bNi cCu d (在式中,a和b分别为Zr,Ti,Ni和Cu原子%,表示c和d,48 a 60、20 b 28、19 c + d 30、3 d 12和0.12

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号