The high glossy natural alloy color development anodic oxidation aluminum material, production manner and the compound aluminum material null which is used for

机译:高光泽天然合金显色阳极氧化铝材料,生产方式及用于

摘要

PROBLEM TO BE SOLVED: To obtain a self-developing alloy having a high glossy feeling, and to reduce an environmental load through the reduction of smut.;SOLUTION: A transparent anodization-treated coating is formed on a colored self developing anodization-treated coating. Concretely, to a composite aluminum material obtained by forming an external layer material composed of pure aluminum with a substantially uniform thickness of 1 to 10 μm and a purity of ≥99.6% on the surface of at least one side in an aluminum alloy internal layer material having colored self-developing, an anodization-treated coating with a thickness of ≥2 times that of the external layer material is formed. As the internal layer material, an Al-Mn based alloy comprising 1.1 to 2.5% Mn, an Al-Si based alloy comprising 2 to 15% Si or the like can be cited.;COPYRIGHT: (C)2006,JPO&NCIPI
机译:解决的问题:获得具有高光泽感的自显影合金,并通过减少黑斑来减少环境负荷。解决方案:在有色自显影阳极氧化处理的涂层上形成透明的阳极氧化处理涂层。具体而言,是通过在铝合金的至少一侧的表面上形成由均匀厚度为1〜10μm,纯度为99.6%以上的纯铝构成的外层材料而得到的复合铝材料。内层材料具有彩色自显影性,形成厚度为外层材料厚度的2倍的阳极氧化处理涂层。作为内层材料,可以列举出含有1.1〜2.5%的Mn的Al-Mn系合金,含有2〜15%的Si的Al-Si系合金等。版权所有:(C)2006,JPO&NCIPI

著录项

  • 公开/公告号JP4629988B2

    专利类型

  • 公开/公告日2011-02-09

    原文格式PDF

  • 申请/专利权人 古河スカイ株式会社;

    申请/专利号JP20040086074

  • 发明设计人 鈴木義和;

    申请日2004-03-24

  • 分类号C25D11/04;C22C21/00;C22F1/04;C22F1/00;

  • 国家 JP

  • 入库时间 2022-08-21 18:16:45

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号