The invention relates to a process for treating cloths made of carbon, Kevlar or carbon-Kevlar fibres to be used for manufacturing composite polymeric boards. According to the invention, the process consists in washing the extended cloth by pulverization of a 30% surface-active solution, degreasing the same by pulverization of a 20% sodium hydroxide solution, rinsing with water jet, drying naturally for 24 h, at the ambient temperature, applying by pulverization a solution of 30% hypochlorite, followed by natural drying for 1 h, applying by pulverization a solution of 20% polybutadiene rubber addittivated with 6% alumino-silicate and 6% amorphous carbon, followed by natural drying for 2 h, applying by pulverization a component A - epoxy resin precursor addittivated with 6% alumino-silicate and 6% amorphous carbon, followed by natural drying for 2 h, applying by pulverization a component B - amine precursor addittivated with 6% alumino-silicate and 6% amorphous carbon, followed by a final natural drying for 24 h at the ambient temperature.
机译:本发明涉及一种处理由碳,凯夫拉尔纤维或碳-凯夫拉尔纤维制成的布的方法,该布用于制造复合聚合物板。根据本发明,该方法包括通过将30%的表面活性溶液粉碎来洗涤延伸的布,通过将20%的氢氧化钠溶液粉碎来对其进行脱脂,用水冲洗,自然干燥24小时。在室温下,先将30%次氯酸盐粉碎,然后自然干燥1 h,再将20%聚丁二烯橡胶粉碎,再加入6%的铝硅酸盐和6%的无定形碳,然后自然干燥2 h,通过粉碎施用组分A-添加有6%铝硅酸盐和6%无定形碳的环氧树脂前体,然后自然干燥2h,通过粉碎施用组分B-添加有6%铝硅酸盐和铝的胺前体。 6%无定形碳,然后在环境温度下自然干燥24小时。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号