A method for plasticity forming of wrought magnesium alloy containing rare earth elements comprises: subjecting the magnesium alloy, obtained by smelting, to heat treatment and peel off treatment; pre-heating it at 200-500℃ for a period from 20 minutes to 2 hours; and subjecting the pre-heated magnesium alloy to extruding, rolling or hot-rolling treatment. The ingredients of the wrought magnesium alloy are: 1.5-3.6wt% of Nd, 0.3-0.6wt% of Zr, 0-0.5wt% of Zn, 0-1.0wt% of heavy metal elements, 0-0.02wt% of impurities, and the balance of Mg. The prepared magnesium alloy has better plasticity and tensile/compression symmetry than traditional wrought magnesium alloy.
机译:一种含有稀土元素的变形镁合金塑性成形的方法,包括:对通过熔炼得到的镁合金进行热处理和剥离处理;在200-500℃下预热20分钟至2小时;对预热的镁合金进行挤压,轧制或热轧处理。变形镁合金的成分为:Nd 1.5-3.6wt%,Zr 0.3-0.6wt%,Zn 0-0.5wt%,重金属元素0-1.0wt%,杂质0-0.02wt% ,其余为Mg。所制备的镁合金比传统的变形镁合金具有更好的可塑性和拉伸/压缩对称性。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号