首页> 外国专利> SLURRY COMPOSITION FOR SOIL IMPROVEMENT CONTAINING BLAST FURNACE SLAG CEMENT AND METHOD FOR PREPARING SOIL CEMENT SLURRY USING SAME

SLURRY COMPOSITION FOR SOIL IMPROVEMENT CONTAINING BLAST FURNACE SLAG CEMENT AND METHOD FOR PREPARING SOIL CEMENT SLURRY USING SAME

机译:含高炉渣水泥的泥浆组合物及其制备方法的研究

摘要

Provided is a slurry composition for soil improvement in which a fine powder of blast furnace slag is used in a higher proportion than in conventional compositions on the premise that a cured soil having necessary strength is obtained while ensuring satisfactory applicability in soil improvement works and which therefore can contribute to a reduction in carbon dioxide emission. Also provided is a method for preparing a soil cement slurry using the composition. The slurry composition for soil improvement is a composition which has been prepared using the blast furnace slag cement described below as a cement, while regulating the mass ratio of water to the blast furnace slag cement to 40-250%, and which further contains an admixture in an amount of 0.1-5 parts by mass per 100 parts by mass of the blast furnace slag cement. Blast furnace slag cement: A blast furnace slag cement composed of a fine powder of blast furnace slag having a fineness of 3,000-13,000 cm2/g and portland cement, the contents of the fine powder of blast furnace slag and the portland cement being 60-80 mass% and 20-40 mass%, respectively (total, 100 mass%).
机译:提供一种用于土壤改良的浆料组合物,其中在确保具有所需强度的固化土壤同时确保在土壤改良工作中令人满意的适用性的前提下,以比常规组合物更高的比例使用高炉矿渣的细粉。可以有助于减少二氧化碳的排放。还提供了使用该组合物制备土壤水泥浆的方法。用于土壤改良的浆料组合物是使用以下所述的高炉矿渣水泥作为水泥制备的组合物,同时将水与高炉矿渣水泥的质量比调节为40-250%,并且还包含掺合料。每100质量份高炉矿渣水泥的量为0.1-5质量份。高炉矿渣水泥:一种高炉矿渣水泥,由细度为3,000-13,000 cm2 / g的高炉矿渣粉和硅酸盐水泥组成,高炉矿渣细粉和硅酸盐水泥的含量为60-分别为80质量%和20-40质量%(总计100质量%)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号