PPROBLEM TO BE SOLVED: To provide a ground-improving slurry composition which ensures good applicability in ground-improving constructions, uses blast furnace slag powder in a higher rate than the present slurry compositions to give ground-cured products having necessary strengths, and can inhibit the generation of carbon dioxide, and to provide a method for preparing a soil cement slurry using the same. PSOLUTION: This ground-improving slurry composition is characterized by using the following blast furnace slag composition as a binder to prepare a water/the blast furnace slag composition in a mass ratio of 40 to 250%, and containing an admixture in an amount of 0.1 to 5 pts.mass per 100 pts.mass of the blast furnace slag composition. The blast furnace slag composition is prepared by adding 0.5 to 1.5 pts.mass or 5 to 45 pts.mass of an alkali stimulating material to 100 pts.mass of a mixture comprising 80 to 95 mass% of blast furnace slag powder having a fineness of 3,000 to 13,000 cmSP2/SP/g and 5 to 20 mass% of gypsum (totally 100 mass%). PCOPYRIGHT: (C)2011,JPO&INPIT
机译:

要解决的问题:为了提供一种能确保在地面改良建筑中良好应用的地面改良泥浆组合物,以比本发明的泥浆组合物更高的比率使用高炉矿渣粉,以获得具有所需强度的地面固化产品,并可以抑制二氧化碳的产生,并提供一种使用该方法制备土壤水泥浆的方法。

解决方案:该地面改良浆料组合物的特征在于,使用以下高炉矿渣组合物作为粘合剂来制备水/高炉矿渣组合物,其质量比为40%至250%,并且在每100 pts高炉渣成分的质量为0.1到5 pts的量。高炉矿渣组合物的制备方法是:向100 pts质量的混合物中加入0.5至1.5 pts.mass或5至45 pts.mass的碱刺激材料,该混合物包含80-95质量%的细度为20的高炉矿渣粉。 3,000至13,000 cm 2 / g和5至20质量%的石膏(总计100质量%)。