Disclosed is a polyethylene resin exhibiting excellent moldability and durability, while having an excellent balance between impact resistance and rigidity.  Also disclosed is a hollow plastic molded article which uses the resin and exhibits excellent moldability, durability and barrier properties, while having an excellent balance between impact resistance and rigidity.  The polyethylene resin satisfies the following conditions (1)-(4).(1) The high-load melt flow rate (HLMFR) is within the range of 1-100 g/10 min.(2) The density is within the range of 0.940-0.960 g/cm3.(3) The strain hardening parameter of elongation viscosity (λmax) is within the range of 1.05-1.50.(4) The rupture time in an all-around notch type tensile creep test and the density satisfy the following formula (A).log (rupture time) ≥ -335 × (density) + 337.6     (A)
机译:公开了具有优异的成型性和耐久性,同时在耐冲击性和刚性之间具有优异的平衡的聚乙烯树脂。还公开了一种中空塑料模塑制品,其使用该树脂并表现出优异的模塑性,耐久性和阻隔性,同时在耐冲击性和刚性之间具有优异的平衡。聚乙烯树脂满足以下条件(1)-(4)。(1)高负荷熔体流动速率(HLMFR)在1-100 g / 10分钟的范围内。(2)密度在0.940-0.960g / cm 3的范围内。(3)延伸粘度的应变硬化参数(λmax)在1.05-1.50的范围内。(4)全方位切口型拉伸蠕变试验的断裂时间和密度满足下式(A)。log(破裂时间)≥-335×(密度)+ 337.6(A)

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号