A polyethylene based resin exhibiting excellent moldability and durability and having an excellent balance between impact resistance and stiffness; and a hollow plastic molded article using the foregoing resin, which exhibits excellent moldability, durability and barrier properties and has an excellent balance between impact resistance and stiffness, are provided. The polyethylene based resin satisfies the following requirements (1) to (4): (1) a high-load melt flow rate (HLMFR) is from 1 to 100 g/10 min; (2) a density is from 0.940 to 0.960 g/cm 3 ; (3) a strain hardening parameter »max of elongational viscosity is from 1.05 to 1.50; and (4) a rupture time in a full notch tensile creep test and a density satisfy the following relational expression (A): log (rupture time) ‰¥ -355 × (density) + 337.6 (A).
机译:聚乙烯基树脂具有优异的成型性和耐久性,并且在耐冲击性和刚性之间具有优异的平衡;本发明提供一种使用上述树脂的中空塑料成型体,该中空塑料成型体显示出优异的成型性,耐久性和阻隔性,并且在耐冲击性和刚性之间具有优异的平衡。聚乙烯基树脂满足以下要求(1)至(4):(1)高负荷熔体流动速率(HLMFR)为1至100g / 10min; (2)密度为0.940至0.960g / cm 3; (3)伸长粘度的应变硬化参数»max为1.05〜1.50。 (4)在全缺口拉伸蠕变试验中的断裂时间和密度满足以下的关系式(A):log(断裂时间)≥-355×(密度)+337.6(A)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号