PURPOSE: A lithium titanium oxide for a positive electrode active material of a lithium rechargeable battery is provided to maximize the yield of lithium titanate with little impurities and to reduce operation costs by obtaining lithium titanate at a lower reaction temperature.;CONSTITUTION: A lithium titanium oxide for a positive electrode active material of a lithium rechargeable battery has a first peak of Li4Ti5O12 peak and a second peak of TiO2 in XRD spectrum, wherein I_(TiO2)/I_(Li4Ti5O12) of the intensity(I_(Li4Ti5O12)) of the first peak and the intensity(I_(TiO2)) of the second peak is 10^(-4) or more and 10^(-1) or less. An XRD analysis condition is 5 ~ 80 °C, 0.02 °C/step and X-ray: 40 kV/20mA.;COPYRIGHT KIPO 2011
机译:用途:提供用于锂可再充电电池的正极活性材料的锂钛氧化物,以最大程度地提高含少量杂质的钛酸锂的产量,并通过在较低的反应温度下获得钛酸锂来降低运营成本。用于锂可充电电池的正极活性材料的氧化物在XRD光谱中具有Li4Ti5O12峰的第一峰和TiO2的第二峰,其中I_(TiO2)/ I_(Li4Ti5O12)的强度(I_(Li4Ti5O12))为第一峰,第二峰的强度(I_(TiO2))为10 ^(-4)以上且10 ^(-1)以下。 XRD分析条件为5〜80°C,0.02°C /步且X射线:40 kV / 20mA。; COPYRIGHT KIPO 2011

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号