1. A method of producing shells on the basis of chitosan and alginic acid salts for microcapsules containing phospholipid micelles, characterized sequential exposure microcapsule cores in 0,5 ÷ 1,0% (wt. / Vol.) Solution of chitosan medium or low viscosity 1.0 % acetic acid at 2.5 ÷ 3.0% solution of alkaline earth metal chloride, a 0.5 ÷ 1.0% (wt. / vol.) sodium alginate solution and, again, a 2.5 ÷ 3.0% alkaline earth metal chloride solution. ! 2. A method according to claim 1, characterized in that the microcapsules are kept in a chitosan solution 25 ÷ 30 minutes, a solution of an alkaline earth metal chloride, - at least 25 ÷ 30 minutes, a solution of sodium alginate - at least 5 ÷ 10 minutes, again in a solution alkaline earth metal chloride, - at least 10 ÷ 15 minutes. ! 3. A method according to claim 1, characterized in that the alkaline earth metal chloride, calcium chloride is used. ! 4. A method according to claim 1, characterized in that the alkaline earth metal chloride is used barium chloride.
机译:1.一种基于壳聚糖和海藻酸盐的用于制备包含磷脂微团的微胶囊的壳的方法,其特征在于,以0.5÷1.0%(重量/体积)的壳聚糖溶液在中等或低粘度的溶液中连续暴露微胶囊核。在碱土金属氯化物的2.5÷3.0%的溶液中加入1.0%的乙酸,在海藻酸钠溶液中的0.5÷1.0%(wt./vol。)的海藻酸钠溶液和2.5÷3.0%的碱土金属氯化物的溶液。 ! 2.根据权利要求1所述的方法,其特征在于,将所述微胶囊在壳聚糖溶液中保存25〜30分钟,在碱土金属氯化物的溶液中至少25〜30分钟,在藻酸钠溶液中-至少再次在碱土金属氯化物溶液中5到10分钟-至少10到15分钟。 ! 3.根据权利要求1的方法,其特征在于使用碱土金属氯化物氯化钙。 ! 4.根据权利要求1所述的方法,其特征在于,所述碱土金属氯化物使用氯化钡。

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号