首页> 外国专利> ALL-ANTIFRICTION NANOSTRUCTURED wear resistance dampens the shape memory alloy on METASTABLE BASED IRON STRUCTURE GEKSANALNOGO ε-martensite AND ARTICLES USING THESE ALLOYS WITH EFFECT SELF NANOSTRUCTURAL Compositions, self-strengthening and self-lubricating friction surfaces EFFECT self-extinguishing vibration and noise

ALL-ANTIFRICTION NANOSTRUCTURED wear resistance dampens the shape memory alloy on METASTABLE BASED IRON STRUCTURE GEKSANALNOGO ε-martensite AND ARTICLES USING THESE ALLOYS WITH EFFECT SELF NANOSTRUCTURAL Compositions, self-strengthening and self-lubricating friction surfaces EFFECT self-extinguishing vibration and noise

机译:全抗纳米结构的耐磨性可抑制亚稳态GESSANALNOGOε-马氏体的亚稳态铁结构和使用这些具有有效纳米结构,自增强和自润滑摩擦表面的合金的形状记忆合金

摘要

FIELD: metallurgy.;SUBSTANCE: alloy contains the following, wt %: carbon 0.001 - 0.3, manganese 5.0 - 44.0, nitrogen 0.03 - 0.12, and iron is the rest; at that, its structure contains 5 - 95% of ε-martensite phase, and γ-austenite and/or α-martensite is the rest. Alloy can also contain 0.5 - 8.0 wt % of silicium and/or cobalt and one or several elements of the group: titanium 0.06 - 1.0, vanadium 0.06 - 0.20 and niobium 0.05 - 0.20.;EFFECT: alloy has high damping and antifriction properties, wear resistance and shape memory effect, which allows using it for manufacture of items having the effect of self-organisation of nanostructure compositions on intense friction surfaces, effect of self-strengthening, self-lubrication, self-damping of vibrations and noises, which are used for operation at normal and negative temperatures.;9 cl, 13 dwg, 4 tbl
机译:领域:冶金;物质:合金包含以下重量百分比:碳0.001-0.3,锰5.0-44.0,氮0.03-0.12,其余为铁;那时,它的结构包含5-95%的ε-马氏体相,其余为γ-奥氏体和/或α-马氏体。合金还可以包含0.5-8.0 wt%的硅和/或钴以及一种或几种元素:钛0.06-1.0,钒0.06-0.20和铌0.05-0.20;效果:合金具有高阻尼和减摩性能,耐磨性和形状记忆效应,使其可用于制造具有在强摩擦表面上自组织纳米结构组合物,自增强,自润滑,振动和噪声自阻尼的效果的物品。用于在正常温度和负温度下运行; 9 cl,13 dwg,4 tbl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号