A continuous electroforming process to form a strip for battery electrodes, comprising the steps of providing a mandrel having on its surface a reusable pattern subdivided into conductive and non-conductive areas; moving said mandrel through an electroforming bath to deposit a metal layer on said mandrel while it moves through the electroforming bath until the metal layer has assumed the shape of the conductive pattern and a thickness at least sufficient to provide strength for the layer to be removed from said mandrel; and separating said layer from said mandrel; is characterised by moving said strip through at least one subsequent bath in which electrodeposition of metal takes place on both sides of said strip while it is moved through said subsequent bath, applying a current density of at least 10 A/dm2 and up to 300 A/dm2 to the conductive surface of the moving mandrel and to the metal surface of the strip in each of the subsequent baths; and directing a forced flow of electrolyte onto the surface of the layer and said strip, wherein the reusable conductive pattern of the surface of the mandrel takes the form of at least one battery electrode and the electrolyte contains additives providing increased hardness, increased corrosion resistance and being suited specifically to permit combining a high rate of deposition with controlled surface roughness and controlled composition of the deposit. IMAGE
机译:一种用于形成电池电极条的连续电铸工艺,包括以下步骤:提供芯棒,在芯棒的表面上具有可重复使用的图案,该图案可细分为导电和非导电区域;使所述心轴移动通过电铸浴,以在所述心轴移动通过电铸浴时在其上沉积金属层,直到金属层呈现出导电图案的形状和厚度至少足以为要从其上去除的层提供强度为止心轴说将所述层与所述心轴分离;其特征在于,使所述带穿过至少一个随后的浴,其中,当金属通过所述随后的浴时,在所述带的两侧进行电沉积,施加至少10A / dm 2的电流密度以上。在每个随后的熔池中,相对于移动芯轴的导电表面以及相对于带材的金属表面的相对电流为300 A / dm 2;以及将电解质强制流引导到所述层和所述条的表面上,其中所述心轴表面的可重复使用的导电图案采用至少一个电池电极的形式,并且所述电解质包含添加剂,所述添加剂提供增加的硬度,增加的耐腐蚀性和特别适合于使高沉积速率与受控的表面粗糙度和受控的沉积物组合相结合。 <图像>

著录项

  • 公开/公告号DE60238106D1

    专利类型

  • 公开/公告日2010-12-09

    原文格式PDF

  • 申请/专利权人 DSL DRESDEN MATERIAL INNOVATION GMBH;

    申请/专利号DE20026038106T

  • 发明设计人 WARLIMONT HANS;

    申请日2002-01-16

  • 分类号C25D1;C25D1/04;C25D1/08;H01M4/04;H01M4/64;H01M4/74;

  • 国家 DE

  • 入库时间 2022-08-21 17:46:14

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号