SULFURIC ACID DEW POINT CORROSION RESISTANT STEEL AND EXHAUST GAS FLOW-PATH CONSTRUCTIONAL ELEMENT

机译:耐硫酸露点耐腐蚀钢和排烟气的流道结构要素

摘要

PROBLEM TO BE SOLVED: To improve a sulfuric acid dew point corrosion resistant property without depending on Sb addition in a steel with an ordinary steel as a basis.;SOLUTION: The sulfuric acid dew point corrosion resistant steel is composed of, by mass, 0.005 to 0.200% C, 0.01 to 0.80% Si, 0.03 to 1.50% Mn, 0.002 to 0.020% P, 0.001 to 0.015% S, 0.10 to 0.50% Cu, 0.05 to 0.30% Ni, 0 to 0.30% Cr, 0.010 to 0.030% Mo, 0.005 to 0.100% Al, and the balance Fe with impurities. The steel is useful especially as a burnt exhaust gas flow-path constructional element in a coal-burning thermal power plant.;COPYRIGHT: (C)2012,JPO&INPIT
机译:解决的问题:以普通钢为基础,不依赖于添加Sb的情况下,提高耐硫酸露点腐蚀性能。解决方案:耐硫酸露点腐蚀钢的质量分数为0.005至0.200%C,0.01至0.80%Si,0.03至1.50%Mn,0.002至0.020%P,0.001至0.015%S,0.10至0.50%Cu,0.05至0.30%Ni,0至0.30%Cr,0.010至< Mo为0.030%,Al为0.005至0.100%,其余为Fe和杂质。该钢尤其可用作燃煤热电厂的燃烧废气流路结构元件。;版权所有:(C)2012,JPO&INPIT

著录项

  • 公开/公告号JP2012180546A

    专利类型

  • 公开/公告日2012-09-20

    原文格式PDF

  • 申请/专利权人 NISSHIN STEEL CO LTD;

    申请/专利号JP20110043183

  • 发明设计人 FUJIWARA SUSUMU;KATAGIRI YUKIO;

    申请日2011-02-28

  • 分类号C22C38/00;C22C38/44;

  • 国家 JP

  • 入库时间 2022-08-21 17:44:18

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号