PROBLEM TO BE SOLVED: To achieve a simultaneous improvement of a sulfuric acid dew-point corrosion resistance and hydrochloric acid dew-point corrosion resistance without relying on Sb-addition, in a steel based with an ordinary steel.;SOLUTION: The acid dew-point corrosion resistant steel is composed, by mass%, of 0.010-0.060% C, ≤0.50% Si, ≤1.50% Mn, ≤0.025% P, ≤0.025% S, 0.10-0.50% Cu, ≤0.30% Ni, 0.10-0.25% Cr, 0.03-0.07% Mo, ≤0.100% Al and the balance Fe, and impurities. The steel is useful as a flow path structure member of especially combustion exhausting gas in a coal-combustion thermal-power plant or the combustion exhausting gas in a waste material incinerating facility.;COPYRIGHT: (C)2012,JPO&INPIT
机译:解决的问题:在不依赖于Sb的情况下,在普通钢基钢中同时提高耐硫酸露点腐蚀性能和耐盐酸露点腐蚀性能;解决方案:点耐蚀钢按质量百分比由0.010-0.060%C,≤0.50%Si,≤1.50%Mn,≤0.025%P,≤0.025%S,0.10-0.50%Cu,≤0.30%Ni,0.10组成-0.25%Cr,0.03-0.07%Mo,≤0.100%Al和余量的Fe和杂质。这种钢特别适合用作燃煤热电厂的燃烧废气或废物焚烧设施中的燃烧废气的流路结构构件。版权所有:(C)2012,JPO&INPIT

著录项

  • 公开/公告号JP5818418B2

    专利类型

  • 公开/公告日2015-11-18

    原文格式PDF

  • 申请/专利权人 日新製鋼株式会社;

    申请/专利号JP20100202518

  • 发明设计人 藤原 進;片桐 幸男;藤本 延和;

    申请日2010-09-09

  • 分类号C22C38/00;C22C38/44;

  • 国家 JP

  • 入库时间 2022-08-21 14:40:35

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号