PROBLEM TO BE SOLVED: To provide an asphalt mixture for a thin layer pavement and a method of repairing a pavement surface using the same by which an existing pavement surface can be paved with a thin layer to have sufficient strength and durability.;SOLUTION: An asphalt mixture for a thin layer pavement uses an aggregate which has a maximum particle diameter of 4.75-5 mm and in which the passage weight percentage at a particle diameter of 2.36 mm is 45-65%. The asphalt mixture uses modified asphalt produced by adding and mixing a modifier, mainly composed of paraffin-based hydrocarbon produced by burning of polymer-based synthetic resin materials having self-burning performance at a softening point of 100-120°C, to and with the asphalt at a compounding ratio of 3-10 wt.%. The asphalt mixture is provided by adding the modified asphalt at a compounding ratio of 6-8 wt.% and heating and mixing it with the aggregate.;COPYRIGHT: (C)2012,JPO&INPIT
机译:解决的问题:提供一种用于薄层路面的沥青混合料以及一种使用该沥青混合料修复路面的方法,通过该方法可以在现有路面上铺上一层薄薄的沥青以具有足够的强度和耐久性。用于薄层路面的沥青混合料使用最大粒径为4.75-5mm的骨料,其中在2.36mm粒径下的通过重量百分比为45-65%。沥青混合物使用改性沥青,该改性沥青通过添加和混合主要由具有自燃性能的聚合物基合成树脂材料在软化点为100至12℃下燃烧而生成的主要由石蜡基烃组成的改性剂制成,沥青的混合比为3-10重量%。通过以6-8 wt。%的混合比添加改性沥青并加热并将其与骨料混合来提供沥青混合物。;版权所有:(C)2012,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号