The present invention relates to a composite electrode material having a carbon base material and iron oxide particles mainly containing Fe3O4 and being supported on the carbon base material and the particles have a D90 of 50 nm or less. In the composite electrode material, since the particle size of the iron oxide particles mainly containing Fe3O4 serving as an active material is small, the electron conductivity of the composite electrode material is not considerably reduced even when being covered with a Fe(OH)2 layer as a reactive intermediate for an electrode reaction. Thus, when the composite electrode material is used, an iron negative electrode having sufficient electron conductivity and charge-discharge cycle characteristics is provided. A negative electrode including the composite electrode material is favorably used as a negative electrode for a metal-air battery.
机译:复合电极材料技术领域本发明涉及一种复合电极材料,其具有碳基材和主要包含Fe 3 O 4 的氧化铁颗粒,并被负载在所述碳基材上,并且所述颗粒具有D 90 等于或小于50 nm。在复合电极材料中,由于主要包含作为活性物质的Fe 3 O 4 的氧化铁粒子的粒径小,因此复合电极的电子传导率即使被Fe(OH) 2 层覆盖作为电极反应的反应性中间体,该材料也不会显着降低。因此,当使用复合电极材料时,提供了具有足够的电子传导性和充放电循环特性的铁负极。包含复合电极材料的负极有利地用作金属-空气电池的负极。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号