Positive Electrode active material for non-aqueous electrolyte-based secondary battery, production method therefor and non-aqueous electrolyte-based secondary battery using the same

机译:用于非水电解质基二次电池的正极活性材料,其制备方法和使用其的非水电解质基二次电池

摘要

The present invention provides a positive electrode active material for a non-aqueous electrolyte-based secondary battery, composed of a lithium/nickel composite oxide with high capacity, low cost and excellent heat stability, an industrially suitable production method therefor, and a high safety non-aqueous electrolyte-based secondary battery. A lithium/nickel composite oxide is produced by the following steps (a) to (c):(a) Nickel hydroxide or nickel oxyhydroxide having a specified component is prepared at a temperature of 600 to 1100° C., under air atmosphere.(b) Fired powders are prepared after mixing said nickel oxide and a lithium compound, and then by firing at a maximal temperature range of 650 to 850° C., under oxygen atmosphere.(c) Obtained fired powders are washed with water within a time satisfying the following equation (2) and then filtered and dried.A≦B/40   (2)wherein, A represents washing time represented by unit of minute; and B represents slurry concentration represented by unit of g/L).
机译:本发明提供由高容量,低成本和优异的热稳定性的锂/镍复合氧化物构成的非水电解质类二次电池用正极活性物质,其工业上适合的制造方法以及高安全性。非水电解质基二次电池。通过以下步骤(a)至(c)制备锂/镍复合氧化物: (a)具有特定成分的氢氧化镍或羟基氧化镍是在600至1100°C的空气氛围中制备的。 (b)在将所述氧化镍和锂化合物混合之后,然后通过在氧气气氛下在最高温度范围为650至850℃下烧制来制备烧成粉末。 A≦B / 40(2)<?in-line-formulae description =“在线公式“ end =“ tail”?>其中,A表示以分钟为单位的洗涤时间; B表示以g / L为单位的浆料浓度。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号