A METHOD FOR IMPROVING THE LIQUEFACTION RESISTANCE OF POND ASH DEPOSITS

机译:一种提高粉煤灰沉积物液化能力的方法

摘要

This invention relates to a method for improving the liquefaction resistance of pond ash deposits using stone-sand columns comprising essentially the steps, providing a device having a casing pipe with a detachable shoe and a hammer; driving the casing pipe with detachable shoe at the bottom of the deposit by the hammer at a desired location to create a hole; filling the casing pipe upto a first depth with a desired back fill material; withdrawing or lifting the casing pipe from the bottom of the surface; compacting the back fill material inside the hole by adapting the dynamic compaction method; repeating the steps (b) to (e) for achieving a maximum compaction; filling the casing pipe upto a second depth with the desired back fill material; and repeating the steps (b) to (g) layer wise till the compaction piles are installed up to the existing ground level. Wherein the stone sand columns decrease the time for building up of maximum pore pressure, the duration for which maximum pore pressure stays and total time for dissipation of pore water pressure resulting in decrease in drainage path, thus reducing the liquefaction potential.
机译:本发明涉及一种使用石砂柱改善池塘灰沉积物抗液化性的方法,主要包括以下步骤:提供一种具有套管的装置,该套管带有可拆卸的靴子和锤子。在所需位置用锤子在沉积物的底部用可脱卸的靴子驱动套管。用期望的回填材料将套管填充到第一深度;从地面底部抽出或提起套管;通过采用动态压实方法压实孔内的回填材料;重复步骤(b)至(e)以达到最大压实度;用所需的回填材料将套管填充到第二个深度;并逐层重复步骤(b)至(g),直到压实桩安装到现有地面为止。其中,石砂柱减少了最大孔隙压力的建立时间,最大孔隙压力保持的持续时间和孔隙水压力消散的总时间导致了排水路径的减少,从而降低了液化潜力。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号