[PROBLEMS] provides transfer fluoro-rubber composite, be not exposed in this way the extrusions talcum bloomed in heat-resisting, low temperature resistant, colorable fluorubber and can provide product with same function and material that conventional batch produces and its to significantly reduce rejection rate prepare raw material; With manufacture crosslinked fluororubber. [MEANS FOR SOLVING PROBLEMS] composition is comprising the fluorubber as necessary component by the fluoropolymer of peroxide cure, peroxide crosslinking agent, heat-resistant filler includes that calcination of talc has water-wetted surface, it is characterized in that the calcination of talc is preferably value -40 of the low form ternary fluoropolymer with TR10 to -25 °C for the fluoropolymer of 2 to 20 parts by weight, 100 parts by weight fluoropolymer and this peroxide cure, it is still preferred to vinylidene fluoride/perfluor (methyl vinyl ether)/tetrafluoroethylene terpolymers.
机译:[问题]提供了转移性氟橡胶复合材料,不会以这种方式暴露挤出的滑石粉在耐热,耐低温,可着色的氟橡胶中起霜,并且可以提供具有与常规批生产相同的功能和材料的产品,并显着减少废品率率准备原料;与制造交联的氟橡胶。 [用于解决问题的方法]组合物包含由过氧化物固化的含氟聚合物作为必需成分的氟,过氧化物交联剂,耐热性填料,其中所述滑石的煅烧具有水润湿的表面,其特征在于所述滑石的煅烧为水。对于2至20重量份的含氟聚合物,100重量份的含氟聚合物和过氧化物固化,TR10至-25°C的低形态三元含氟聚合物的值优选为-40,并且该过氧化物固化时,仍然优选偏二氟乙烯/全氟(甲基乙烯基醚)/四氟乙烯三元共聚物。

著录项

  • 公开/公告号EP2070981B1

    专利类型

  • 公开/公告日2012-02-29

    原文格式PDF

  • 申请/专利权人 NOK CORP;

    申请/专利号EP20070807574

  • 发明设计人 SANO HIROYUKI;

    申请日2007-09-19

  • 分类号C08L27/12;C08K3/34;C08K9/02;

  • 国家 EP

  • 入库时间 2022-08-21 17:16:38

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号