METHOD FOR MANUFACTURING A CERAMIC COATING LAYER FOR IMPROVING ABRASION-RESISTANCE OF A METAL THROUGH AEROSOL EVAPORATION, AND A CERAMIC COATING LAYER OF METAL USING THE SAME

机译:制造通过气溶胶蒸发改善金属耐磨性的陶瓷涂层的方法以及使用该涂层的金属陶瓷涂层

摘要

PURPOSE: A method for manufacturing a ceramic coating layer for improving abrasion-resistance of a metal is provided to can obtain additional functions without abrasion-resistant effect by evaporating ceramic powder on one selected from titanium dioxide, aluminum oxide and yttria-stabilized zirconia.;CONSTITUTION: A method for manufacturing a ceramic coating layer for improving abrasion-resistance of a metal comprises: a step of preparing a metal substrate; a step of heat-treating the ceramic powder at constant temperature; a step of forming a ceramic coating layer by evaporating through aerosol evaporation of the ceramic powder on the metal substrate. The ceramic powder is one selected from titanium dioxide(TiO2), aluminum oxide(Al2O3), yttria-stabilized zirconia, and ceria(CeO2). The metal substrate consists of one selected from magnesium or magnesium alloy, aluminum or aluminum alloy, carbon steel, and stainless steel. The heat treatment is conducted at the temperature of 500-700 °C, for 1-5 hours.;COPYRIGHT KIPO 2012
机译:目的:提供一种用于提高金属的耐磨性的陶瓷涂层的制造方法,该方法可以通过在选自二氧化钛,氧化铝和氧化钇稳定的氧化锆中的一种上蒸发陶瓷粉末而获得没有耐磨性的附加功能。构成:一种用于提高金属的耐磨性的陶瓷涂层的制造方法,包括:准备金属基板的步骤;在恒定温度下热处理陶瓷粉的步骤;通过在金属基板上通过气溶胶蒸发陶瓷粉末而蒸发来形成陶瓷涂层的步骤。陶瓷粉末是选自二氧化钛(TiO 2),氧化铝(Al 2 O 3),氧化钇稳定的氧化锆和二氧化铈(CeO 2)中的一种。金属基底由选自镁或镁合金,铝或铝合金,碳钢和不锈钢中的一种构成。热处理在500-700℃的温度下进行1-5小时。; COPYRIGHT KIPO 2012

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号