A method for preparing terpolymer of poly (biphenyl sulfone ether) and poly (ether sulfone) comprises: adding high-temperature organic solvent into a flask, stirring and heating to 80°C, adding 4,4'-dichlorodiphenylsulfone,4,4'-Bis(4-chlorophenyl)sulionyl-1,1'-biphenyl and 4,4'-dihydroxydiphenylsulfone with solid content of 20-35%; stirring until monomers are completely dissolved, heating to 100°C, adding salt-forming agent and xylene; stirring while heating so that salt-forming reaction begins in the system, wherein the system temperature is controlled between 190°C and 210°C; when the amount of water discharged reaches the theoretical value, the first stage of salt-forming reaction is finished; heating the system to 230-236°C, and maintaining for 3-4 hours to obtain polymer viscous liquid; and refining the polymer viscous liquid to obtain a terpolymer containing different structural units in the molecular chain, wherein the Tg of the terpolymer, can be regulated by changing the ratio of the two dichloro-containing monomers.
机译:一种制备聚(联苯砜醚)和聚(醚砜)三元共聚物的方法,该方法包括:向烧瓶中加入高温有机溶剂,搅拌并加热至80℃,加入4,4′-二氯二苯砜,4,4′。 -固含量为20-35%的双(4-氯苯基)磺酰基-1,1′-联苯和4,4′-二羟基二苯砜;搅拌直至单体完全溶解,加热至100℃,加入成盐剂和二甲苯。边加热边搅拌,使体系中开始成盐反应,体系温度控制在190℃至210℃之间。当排出的水量达到理论值时,成盐反应的第一阶段完成。将系统加热至230-236℃,并保持3-4小时以获得聚合物粘性液体。提纯聚合物粘稠液体以获得在分子链中包含不同结构单元的三元共聚物,其中三元共聚物的Tg可通过改变两种含二氯单体的比例来调节。

著录项

  • 公开/公告号KR20120098593A

    专利类型

  • 公开/公告日2012-09-05

    原文格式PDF

  • 申请/专利权人 KINGFA SCI. & TECH. CO. LTD.;

    申请/专利号KR20127005482

  • 发明设计人 WU ZHONGWEN;MA RONGTANG;

    申请日2010-10-26

  • 分类号C08G75/20;C08G75/23;C08L81/06;

  • 国家 KR

  • 入库时间 2022-08-21 17:09:15

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号