首页> 外国专利> MANUFACTURING METHOD OF ALKALINE IONIZED WATER AND PROCESSED LOESS MATERIALS CAPABLE OF ENHANCING VIRUS ANTISEPTIC EFFECTS, ANTI-CORROSIVE EFFECTS

MANUFACTURING METHOD OF ALKALINE IONIZED WATER AND PROCESSED LOESS MATERIALS CAPABLE OF ENHANCING VIRUS ANTISEPTIC EFFECTS, ANTI-CORROSIVE EFFECTS

机译:碱性离子水和加工黄土材料的制造方法,可增强病毒的对映体作用,抗腐蚀作用

摘要

PURPOSE: A manufacturing method of alkaline ionized water and processed loess materials is provided to reduce manufacturing costs by reducing reaction temperature and time.;CONSTITUTION: A manufacturing method of alkaline ionized water and processed loess materials comprises the following steps: obtaining a mixed composition by mixing 90-10 parts by weight of NaOH based on 10-90 parts by weight of loess ; obtaining liquid molten products by heating the mixed composition at 1100-1300 deg. Celsius for 1-4 hours; and cooling the molten products; pulverizing the cooled material into micro sized or nano sized particles; and extracting the crushed material at 100-150 deg. Celsius for 1-5 hours by adding the same into water.;COPYRIGHT KIPO 2013;[Reference numerals] (AA) Loess; (BB) Mixing sodium hydroxide; (CC) Fusing the mixture (1100-1300 deg. Celsius, 1-4 hours); (DD) Cooling the fused material; (EE) Pulverizing (micro particle, nano particle); (FF) Alkali ionized water(100-150 deg. Celsius, extracting 1-5 hours)
机译:目的:提供一种碱性离子水和经处理的黄土材料的制造方法,以通过降低反应温度和时间来降低制造成本。组成:一种碱性离子水和经处理的黄土材料的制造方法包括以下步骤:基于10-90重量份黄土混合90-10重量份NaOH;通过在1100-1300℃下加热混合的组合物获得液态熔融产物。摄氏1-4小时;冷却熔融产品;将冷却的材料粉碎成微米或纳米尺寸的颗粒;并在100-150度下提取碎料。 COPYRIGHT KIPO 2013; [参考数字](AA)黄土; (BB)混合氢氧化钠; (CC)将混合物熔融(1100-1300℃,1-4小时); (DD)冷却熔融材料; (EE)粉碎(微粒,纳米粒子); (FF)碱水(100-150摄氏度,萃取1-5小时)

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号