FIELD: construction.;SUBSTANCE: method to prepare a concrete mixture for manufacturing of a ballast pipe includes mixing of a sulfate-resistant portland cement, heavy spar ore, a plasticising additive on the basis of polycarboxylate ether and water at the following ratio of the components, in wt %: sulfate resistant portland cement 12 -17, water 4-10, plasticising additive on the basis of polycarboxylate ether 0.1- 0.25, heavy spar ore - balance, at the following content of heavy spar ore fractions in wt %: coarse 3-25 mm 7 - 18, fine 0.16 mm - 3 mm 70 - 85, very fine 0.01-0.16 mm 7 - 16, and tempering water of the concrete mixture is previously processed, sending through the magnetic field, where intensity is maintained with the value of 120000 -140000 A/m, with the speed of 0.5 -3.0 m/s, at the same time the water treatment time makes at least 2 hours. The device for preliminary treatment of the concrete mixture tempering water for manufacturing of a ballast pipe comprises a reservoir for water storage, with inlet and outlet nozzles, and a unit of tempering water treatment, the outlet nozzle of the reservoir is connected with the inlet of the tempering water treatment unit arranged in the form of a hollow extended element, inside of which there is permanent magnet with formation of a gap with the inner wall of the hollow extended element, the value of which makes 3 -5 mm, at the same time the permanent magnet has the intensity of the magnetic field of 120000 -140000 A/m, the outlet of the tempering water treatment unit is connected to the inlet nozzle of the reservoir, the outlet of the tempering water treatment unit is connected with the inlet nozzle of the reservoir, the reservoir has an opening for water draining. The invention is developed in subclaims of the invention formula.;EFFECT: higher density of a concrete mixture and production of a concrete with increased strength.;6 cl, 2 tbl, 2 dwg
机译:用于制造压载水管的混凝土混合物的方法包括以下步骤:混合抗硫酸盐的硅酸盐水泥,重晶石矿石,基于聚羧酸醚和水的增塑添加剂。成分,以重量%计:耐硫酸盐硅酸盐水泥12 -17,水4-10,基于聚羧酸醚0.1- 0.25的增塑添加剂,重晶石矿石-余量,按重量百分比计,以下重晶石矿石含量如下:粗3-25毫米7-18,细0.16毫米-3毫米70-85,细0.01-0.16毫米7-16,预先处理混凝土混合物的回火水,并通过磁场保持强度数值为120000 -140000 A / m,速度为0.5 -3.0 m / s,同时水处理时间至少要2个小时。用于制造压载水管的混凝土混合物回火水的初步处理装置包括用于储水的储水器,该储水器具有入口和出口喷嘴,以及回火水处理单元,储水器的出口喷嘴与水的入口相连。回火水处理单元以中空延伸元件的形式布置,在该内部具有永久磁铁,该永磁体与中空延伸元件的内壁形成间隙,其值等于3 -5 mm当永磁体的磁场强度为120000 -140000 A / m时,回火水处理单元的出口与水箱的入口喷嘴相连,回火水处理单元的出口与入口水箱的喷嘴,水箱有一个排水孔。本发明是在本发明的从属权利要求中提出的;效果:高密度的混凝土混合物和高强度混凝土的生产。6 cl,2 tbl,2 dwg

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号