The process for preparing a concrete mix for manufacturing a ballast pipe comprises mixing the following components, in mass%: from 12% to 17% - sulphate-resistant Portland cement; from 4% to 10% - water; from 0.1% to 0.25% - plasticizing additive on the basis of polycarboxylate ether; remainder - barite ore. The fractions content of barite ore in mass% is: from 7% to 18% - large fraction with a particle size of from 3 mm to 25 mm; from 70% to 85% - small fraction with a particle size of from 0.16 mm to 3 mm; from 7% to 16% - very small fraction with a particle size of from 0.01 mm to 0.16 mm. The water for mixing the concrete mix is pre-processed by being passed through a gap in which a magnetic H field is maintained. The device for preliminary preparation of mixing water for the manufacture of a ballast pipe has a mixing water processing unit. A permanent magnet is installed inside the water processing unit so as to form a gap with respect to the inner wall of a hollow elongate element.
机译:制备用于制造压载水管的混凝土混合物的方法包括以质量%混合以下组分:-从12%至17%-耐硫酸盐的波特兰水泥;和4%至10%-水;从0.1%到0.25%-基于聚羧酸醚的增塑添加剂;剩余物-重晶石矿石。重晶石矿石的质量分数百分比含量为:7%至18%-粒径为3 mm至25 mm的较大分数; 70%至85%-小颗粒,粒径为0.16 mm至3 mm;从7%到16%-非常小的颗粒,粒径为0.01毫米到0.16毫米。用于混合混凝土混合料的水通过穿过保持磁场H的间隙进行预处理。用于制造压载管的混合水的预备装置具有混合水处理单元。永磁体安装在水处理单元内部,以便相对于中空细长元件的内壁形成间隙。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号