PROBLEM TO BE SOLVED: To continuously cast a round slab of high Cr steel having a Cr content of 2.0-18.0 mass% while preventing an inner face flaw in time of pipe production.;SOLUTION: A method for producing continuous casting round slab uses a sectional circular mold 4 having a diameter on the inner face side ≤400 mm. A casting speed is 0.6-2.4 m/min. After a round slab 9 is perfectly coagulated at a surface temperature of 800-1,100°C, depression wherein a slab depression ratio RED is 10.0-30.0% is applied by one or more pinch rolls, and the round slab 9 is flattened such that the width dimension in the depression direction becomes smaller than the width dimension on a free face side in a direction orthogonal to the depression direction. The flattened slab is vertically depressed from the direction orthogonal to the vertically depressed direction by one or more shaping rolls to shape a section of the slab to a circular section having a prescribed dimension without flattening the slab.;COPYRIGHT: (C)2013,JPO&INPIT
机译:解决的问题:为了连续铸造高Cr钢的圆板坯,其中Cr含量为2.0-18.0质量%,同时防止管材生产时的内表面缺陷。内表面侧直径≤400mm的截面圆形模具4。铸造速度为0.6-2.4m / min。在表面温度为800-1,100℃的条件下使圆板9完全凝结后,通过一个或多个夹送辊施加压下率RED为10.0-30.0%的压板,将圆板9压平,使在与凹陷方向正交的方向上,凹陷方向上的宽度尺寸变得小于自由面侧上的宽度尺寸。用一个或多个成型辊从垂直于垂直方向压下的方向垂直压平平板,以将平板的一部分成型为具有规定尺寸的圆形截面,而无需压平平板.COPYRIGHT:(C)2013,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号