PROBLEM TO BE SOLVED: To provide a denitration catalyst capable of obtaining a highly active catalyst, efficiently processing a nitrogen oxide (NOX) in an exhaust gas, and in particular effectively affecting the processing of exhaust gas generated from a gas-fired boiler and a gas turbine.;SOLUTION: A denitration catalyst including a composite oxide of titanium and tungsten (hereinafter, referred to as a Ti-W composite oxide) or a composite oxide of titanium, silicon, and tungsten (hereinafter, referred to as a Ti-Si-W composite oxide) satisfies the conditions: (1) To measure the desorption amount of ammonia at 250 to 350°C by ammonia temperature rise desorption measurement (NH3-TPD) (L-desorption amount), (2) to measure the desorption amount of ammonia at 450 to 550°C by ammonia temperature rise desorption measurement (NH3-TPD) (H desorption amount), and (3) to set H desorption amount/L-desorption amount at 0.7 to 1.5.;COPYRIGHT: (C)2013,JPO&INPIT
机译:解决的问题:提供一种脱硝催化剂,其能够获得高活性催化剂,有效地处理废气中的氮氧化物(NOX),特别是有效地影响从燃气锅炉和锅炉产生的废气的处理。解决方案:一种脱硝催化剂,其包括钛和钨的复合氧化物(以下称为Ti-W复合氧化物)或钛,硅和钨的复合氧化物(以下称为Ti-W复合氧化物)。 Si-W复合氧化物)满足以下条件:(1)通过氨升温上升解吸测定(NH 3 -TPD)(L-解吸量)来测定250〜350℃的氨的解吸量。 ),(2)通过氨水升温脱附测量(NH 3 -TPD)(H脱附量)测量450至550°C的氨的脱附量,以及(3)设置H脱附量/ L脱附量在0.7到1.5之间;版权:(C)2013,JPO&INPIT

著录项

  • 公开/公告号JP2013193938A

    专利类型

  • 公开/公告日2013-09-30

    原文格式PDF

  • 申请/专利权人 NIPPON SHOKUBAI CO LTD;

    申请/专利号JP20120064551

  • 申请日2012-03-21

  • 分类号C01G41/00;C01B33/12;B01J23/30;B01D53/94;B01J37/03;F01N3/10;

  • 国家 JP

  • 入库时间 2022-08-21 17:02:58

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号