PPROBLEM TO BE SOLVED: To provide a method for adequately carrying out quality assurance for delivering a product to a user, and also to provide a method for manufacturing of a hot-rolled metal strip using the same. PSOLUTION: A cooling-related equipment 26 between a finish-rolling mill 18 of a hot rolling line 100 and a coiler 24 is divided into a first half zone 5 and a second half zone 4. In the first half zone 5, cooling water is supplied, whose water amount density per one surface of a front surface and a rear surface is 0.7 mSP3/SP/mSP2/SP/min and 1.2 mSP3/SP/mSP2/SP/min respectively. In the second half zone 4, cooling water is supplied, whose water amount density per one surface of the front surface and the rear surface is 2.0 mSP3/SP/mSP2/SP/min and 5.0 mSP3/SP/mSP2/SP/min respectively. In this way, the temperature of the hot-rolled metal strip 8 immediately before winding is controlled. In the first half zone 5, in addition thereto, the full width of the hot-rolled metal strip 8 installed at the exit side of the first half zone 5 is fed back to the control of the temperature of the hot-rolled metal strip 8 in the first half zone 5 based on result of temperature measurement by a near-infrared camera 27A capable of photographing a full length or a part of the full length so that the temperature of the hot-rolled metal strip 8 immediately before winding is controlled. PCOPYRIGHT: (C)2010,JPO&INPIT
机译:

要解决的问题:提供一种适当地执行质量保证以将产品交付给用户的方法,并且还提供一种使用该方法制造热轧金属带的方法。解决方案:在热轧生产线100的精轧机18和卷取机24之间的与冷却有关的设备26被分为前半区5和后半区4。在前半区5中,供应冷却水,其正面和背面的一个表面的水量密度分别为0.7 m 3 / m 2 / min和1.2 m 3 / m 2 / min。在后半部区域4中,供给冷却水,该冷却水的正面和背面的每个面的水量密度为2.0m 3 / m 2 / min和5.0 m 3 / m 2 / min。以这种方式,控制紧接在卷绕之前的热轧金属带材8的温度。此外,在第一半区5中,将安装在第一半区5的出口侧的热轧金属带材8的整个宽度反馈给热轧金属带材8的温度控制。根据近红外照相机27A的温度测量结果,通过在第一半区5中的温度,该近红外照相机能够拍摄全长或全长的一部分,从而控制紧接在卷绕之前的热轧金属带材8的温度。

版权:(C)2010,日本特许厅&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号