首页> 外国专利> A method of manufacturing the same, as well as processes for the preparation thereof and chemically strengthened glass and chemically strengthened glass

A method of manufacturing the same, as well as processes for the preparation thereof and chemically strengthened glass and chemically strengthened glass

机译:制造其的方法及其制备方法以及化学强化玻璃和化学强化玻璃

摘要

Suitable properties, ie, to provide a chemically strengthened glass with excellent transmission characteristics foam quality, intensity, of the light, the color tone of the gray system ornaments applications housing and [challenge] electronics. In a molar percentage of display resolution [means] the following oxide basis, of 55-80% SiO 2, 0.25~16% of Al 2 O 3, 0~12% of B 2 O 3, 5~ the 2 O Na 20% 0 to 15% of 2 O K, 0~15% of MgO, 0~15% of CaO, 0~25% and, (Mg, Ca, Sr, Ba, Zn R is) and ZrO 2 ΣRO 0-1%, from 0.01 to 0.2 percent the Co 3 O 4, 0.05~1% of NiO, chemically strengthened glass containing from 0.005 to 3% of Fe 2 O 3. None [Selection Figure]
机译:合适的属性,即提供具有优异的透射特性的化学强化玻璃,其泡沫质量,光的强度,灰色系统的色调装饰应用外壳和电子器件。以显示分辨率的摩尔百分比[表示],以下氧化基准为SiO 2的55-80%, Al 2 O 3的0.25〜16%, B 2 O 3的0〜12% 5〜 2 O的Na 2%0至15%的 2 O K, MgO的0〜15%,CaO的0〜15%,0〜25%以及(Mg,Ca,Sr,Ba,Zn R是)和ZrO 2 ΣRO0-1%,NiO的 Co 3 O 4,0.01%到0.2%,0.05〜1%,化学强化玻璃含有0.005%到3%的NiO Fe 2 O 3。无[选择图]

著录项

  • 公开/公告号JP5234213B1

    专利类型

  • 公开/公告日2013-07-10

    原文格式PDF

  • 申请/专利权人 旭硝子株式会社;

    申请/专利号JP20120203597

  • 发明设计人 山本 宏行;

    申请日2012-09-14

  • 分类号C03C3/085;C03C3/083;C03C3/087;C03C3/091;C03C3/093;C03C3/095;C03C21/00;

  • 国家 JP

  • 入库时间 2022-08-21 16:55:04

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号