A steel for surface hardening for machine structural use which is characterized by containing, in terms of mass %, 0.30-0.60% C, 0.02-2.0% Si, 0.35-1.5% Mn, 0.001-0.5% Al, 0.05-2.0% Cr, 0.001-1.0% Sn, 0.0001-0.021% S, 0.0030-0.0055% N, 0.01-2.0% Ni, 0.01-2.0% Cu, up to 0.030% P, and up to 0.005% O, with the remainder comprising Fe and incidental impurities, the contents of Sn, Cu, Ni, Mn, and S satisfying relationships (1) and (2).; −0.19≦0.12×Sn+Cu−0.1×Ni≦0.15  (1); 60≦Mn/S≦300  (2)
机译:机械结构用表面硬化钢,其特征在于以质量%计包含0.30-0.60%C,0.02-2.0%Si,0.35-1.5%Mn,0.001-0.5%Al,0.05-2.0%Cr ,0.001-1.0%的Sn,0.0001-0.021%的S,0.0030-0.0055%的N,0.01-2.0%的Ni,0.01-2.0%的Cu,高达0.030%的P和0.005%的O,其余包括Fe和附带杂质中,Sn,Cu,Ni,Mn和S的含量满足关系式(1)和(2)。 <?in-line-formulae description =“在线表达式” end =“ lead”?>-0.19≦0.12×Sn + Cu-0.1×Ni≦0.15(1)<?in-line-formulae description =“ In -line Formulae“ end =” tail“?>; <?in-line-formulae description =“在线表达式” end =“ lead”?> 60≦Mn / S≦300(2)<?in-line-formulae description =“在线表达式” end =“尾巴”?>

著录项

  • 公开/公告号US2013180626A1

    专利类型

  • 公开/公告日2013-07-18

    原文格式PDF

  • 申请/专利权人 SUGURU YOSHIDA;

    申请/专利号US201113825521

  • 发明设计人 SUGURU YOSHIDA;

    申请日2011-08-02

  • 分类号C23C8/80;C23C8/02;

  • 国家 US

  • 入库时间 2022-08-21 16:52:07

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号