PURPOSE: A manufacturing method of concrete using a superplasticizer combined with carbon amino silica black is provided to enhance compressive strength, tensile strength, and a coefficient of elasticity for concrete.;CONSTITUTION: A manufacturing method of concrete using a superplasticizer combine with carbon amino silica black uses 0.5-10 wt% of a polycarboxylic acid-based high functional water reducing agent based on binders of concrete. The polycarboxylic acid-based high functional water reducing agent includes 0.1-30 wt% of carbon amino silica black. The silica mole fraction of the carbon amino silica black is 0.1-20 wt%. The replacement rate (W/B) of the concrete is 15-50%. The concrete includes 25-100 wt% of cement, 0-40 wt% of blast furnace slag powder, 0-25 wt% of fly ash, and 0-10 wt% silica fume.;COPYRIGHT KIPO 2013;[Reference numerals] (AA) Compressive strength; (BB) 3 days; (CC) 7 days; (DD) 28 days; (EE) CASB mixing rate(%)
机译:目的:提供一种使用高效减水剂与碳氨基硅石炭黑结合的混凝土制造方法,以提高混凝土的抗压强度,拉伸强度和弹性系数。;组成:使用高效减水剂与碳氨基硅石结合的混凝土制造方法黑色使用基于混凝土粘合剂的0.5-10 wt%的多羧酸基高功能减水剂。所述基于多元羧酸的高功能减水剂包括0.1-30重量%的碳氨基硅黑。碳氨基二氧化硅黑的二氧化硅摩尔分数为0.1-20重量%。混凝土的替代率(W / B)为15-50%。混凝土包括25-100 wt%的水泥,0-40 wt%的高炉矿渣粉,0-25 wt%的粉煤灰和0-10 wt%的硅粉。; COPYRIGHT KIPO 2013; [参考数字]( AA)抗压强度; (BB)3天; (CC)7天; (DD)28天; (EE)CASB混合率(%)

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号