PURPOSE: A manufacturing method of an air electrode is provided to manufacture the air electrode which is capable of reducing overvoltage in an oxygen reduction reaction and oxygen generation reaction, and has an improved charging and discharging performance. CONSTITUTION: A manufacturing method of an air electrode for a lithium/air secondary battery comprises: a first step manufacturing a spinel-structured Mn_1.5Co_1.5O_4 solid solution; a step of dissolving the spinel-structured Mn1.5Co1.5O4 solid solution and a polymer binder into a solvent; and a step of coating a porous metal support with the mixture with the Mn1.5Co1.5O4 solid solution and the polymer binder. The mixture with Mn1.5Co1.5O4 solid solution and polymer binder additionally comprises ketjen black carbon.
机译:目的:提供一种空气电极的制造方法,以制造能够减少氧还原反应和氧生成反应中的过电压并且具有改善的充电和放电性能的空气电极。构成:锂/空气二次电池用空气电极的制造方法,包括:第一步,制备尖晶石结构的Mn_1.5Co_1.5O_4固溶体;将尖晶石结构的Mn1.5Co1.5O4固溶体和聚合物粘合剂溶解在溶剂中的步骤;所述的方法包括:用Mn1.5Co1.5O4固溶体和聚合物粘合剂的混合物涂覆多孔金属载体。具有Mn1.5Co1.5O4固溶体和聚合物粘合剂的混合物还包含科琴黑碳。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号