PURPOSE: A manufacturing method of an indium tin oxide rod is provided to manufacture an indium tin oxide rod with controlled aspect ratio of length and thickness.;CONSTITUTION: A manufacturing method an indium tin oxide rod comprises a step of forming a first mixture by mixing indium precursor, tin precursor, and terephthalte; a step of mixing alcohol into the first mixture, to obtain a second mixture into dimethyl formamide; a step of obtaining precipitation by refluxing the second mixture; a step of washing and drying the precipitation; and a step of heat treating the precipitation. The weight mixing ratio of the alcohol and the dimethyl formamide is 0.1-0.5. The aspect ratio of the indium tin oxide rod is 4-30. The weight mixing ratio of the indium precursor and the tin precursor is 1-5. The weight mixing ratio of the terephthalte and the indium precursor is 0.5-0.8. The reflux reaction is conducted at 80-140 deg. C, and the heat treatment is conducted at 400-800 deg. C.;COPYRIGHT KIPO 2013
机译:目的:提供一种铟锡氧化物棒的制造方法,以制造长度和厚度的纵横比受控制的铟锡氧化物棒。构成:铟锡氧化物棒的制造方法包括通过混合形成第一混合物的步骤铟前体,锡前体和对苯二甲酸;将醇混合到第一混合物中,得到第二混合物成二甲基甲酰胺的步骤;通过回流第二混合物获得沉淀的步骤;洗涤并干燥沉淀物的步骤;和热处理沉淀的步骤。醇与二甲基甲酰胺的重量混合比为0.1〜0.5。铟锡氧化物棒的纵横比为4〜30。铟前体和锡前体的重量混合比为1-5。对苯二甲酸酯与铟前体的重量混合比为0.5〜0.8。回流反应在80-140℃下进行。并在400-800℃进行热处理。 C .;版权KIPO 2013

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号