PURPOSE: A manufacturing method of a micro capsule type quantum dot-polymer is provided to provide a quantum dot-polymer composite having excellent quantum dot dispersity and capable of stably maintaining quantum efficiency for long term. CONSTITUTION: A manufacturing method of a micro capsule type quantum dot-polymer comprises a step of forming a polymer solution by heating a first polymer having a polar functional group in a side chain and a second polymer with a higher molecular weight than that of the first polymer, in a first solvent (S13); a step of forming a mixture by adding a quantum dot dispersion in which quantum dots capped by a capping layer in a second solvent into the polymer solution(S17); and a step of forming a quantum dot-polymer composite in which the quantum dots are dispersed in a polymer matrix by cooling the mixture (S19). [Reference numerals] (S11) Preparing a polymer having a polar functional group in a side chain and a polymer with a higher molecular weight; (S13) Forming a polymer solution by heating the polymer having a polar functional group in a side chain and the polymer with a higher molecular weight than that of the first polymer, in a first solvent; (S15) Preparing a quantum dot dispersion in which quantum dots capped by a capping layer in a second solvent in a second solvent; (S17) Forming a mixture by adding a quantum dot dispersion in the polymer solution; (S19) Forming a quantum dot-polymer composite by cooling the mixture
机译:目的:提供一种微胶囊型量子点聚合物的制造方法,以提供具有优异的量子点分散性并且能够长期稳定地保持量子效率的量子点-聚合物复合物。构成:一种微胶囊型量子点聚合物的制造方法,包括以下步骤:通过加热侧链中具有极性官能团的第一聚合物和分子量比第一分子高的第二聚合物来形成聚合物溶液聚合物,在第一溶剂中(S13);通过将量子点分散体形成混合物的步骤,在该量子点分散体中,由第二溶剂中的覆盖层覆盖的量子点被添加到聚合物溶液中(S17);形成量子点-聚合物复合物的步骤,其中通过冷却混合物将量子点分散在聚合物基质中(S19)。 [S11]制备侧链中具有极性官能团的聚合物和分子量更高的聚合物。 (S13)通过在第一溶剂中加热在侧链中具有极性官能团的聚合物和具有比第一聚合物更高的分子量的聚合物来形成聚合物溶液; (S15)准备在第二溶剂中的第二溶剂中被覆盖层覆盖的量子点的量子点分散体; (S17)通过在聚合物溶液中添加量子点分散液来形成混合物; (S19)通过冷却混合物形成量子点-聚合物复合物

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号