PURPOSE: A manufacturing method of aggregate for pretensioned spun high strength concrete (PHC) piles and a concrete composition for PHC pile manufacturing which uses the same are provided to omit an autoclave process which requires high energy consumption and to replace natural aggregate by using slag which is industrial byproduct generated from an electric steel manufacturing process. CONSTITUTION: A manufacturing method of aggregate for PHC piles comprises the following steps: (100) cooling oxidizing slag by using melted electric furnace which includes electric slag generated during a steel manufacturing process by the electric furnace; (200) crushing oxidizing slags by using the cooled electric furnace; (300) sorting the crushed electric furnace slag by magnetic force by composition of iron; and (400) sieving the sorted electric furnace oxidizing slag. The manufacturing method of aggregate for PHC piles additionally includes the following steps before the cooling step: (510) isolating ferric oxide by adding a reducing agent to the melted electric furnace oxidizing slag; and (520) adding silicon dioxide. [Reference numerals] (110) Between soil cooling; (120) Fan cooling; (130) Granulating mist cooling; (210) Coarse crushing; (220) Crushing; (300,CC) Magnetic separating; (400,DD) Sieving-analysis test; (510) Iron oxide separating; (520) Silicon dioxide adding; (AA) Electric furnace; (BB) Raw material: ion scrap, quicklime, etc.; (EE) Electric furnace oxidizing slag coarse aggregate; (FF) Electric furnace oxidizing slag fine aggregate
机译:目的:提供一种用于预张拉的高强度混凝土(PHC)桩的骨料的制造方法以及使用该方法的用于PHC桩制造的混凝土组合物,从而省去了需要高能耗的高压釜工艺,并通过使用矿渣代替天然骨料。是电工钢制造过程中产生的工业副产品。组成:PHC桩用骨料的制造方法包括以下步骤:(100)使用熔融电炉冷却氧化炉渣,其中包括在电炉的炼钢过程中产生的电渣; (200)使用冷却的电炉破碎氧化渣; (300)利用磁力根据铁的成分对破碎的电炉炉渣进行分选。 (400)筛分分选后的电炉氧化渣。用于PHC桩的骨料的制造方法在冷却步骤之前还包括以下步骤:(510)通过向熔融的电炉氧化渣中添加还原剂来分离三氧化二铁; (520)添加二氧化硅。 [附图标记](110)在土壤冷却之间; (120)风扇冷却; (130)造粒雾冷却; (210)粗碎; (220)压碎; (300,CC)磁分离; (400,DD)筛分分析测试; (510)氧化铁分离; (520)添加二氧化硅; (AA)电炉; (BB)原料:离子废料,生石灰等; (EE)电炉氧化渣粗骨料; (FF)电炉氧化渣细骨料

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号