A method for reducing red scale on the surface of a hot-rolled steel sheet and a method for manufacturing a hot-rolled steel sheet using the same are disclosed. A method for reducing red scale on the surface of a hot-rolled steel sheet according to the present invention re-heats a slab which contains 0.1 weight% or more of silicone (Si) based on the total weight at 1170?ƒ or lower temperatures and subsequently hot-rolls the slab.;COPYRIGHT KIPO 2014;[Reference numerals] (AA) Start;(BB) End;(S110) Reheat a slab;(S120) Hot-roll (FDT: 850~900?ƒ);(S130) Cool and wind (CT: 600~680?ƒ)
机译:公开了一种用于减少热轧钢板表面上的红皮的方法以及使用该方法制造热轧钢板的方法。根据本发明的用于减少热轧钢板表面上的红皮的方法重新加热包含在1170℃或更低温度下基于总重量为0.1重量%或更多的硅酮(Si)的板坯。 COPYRIGHT KIPO 2014; [参考数字](AA)开始;(BB)结束;(S110)再加热一块板;(S120)热轧(FDT:850〜900?ƒ); (S130)凉风(CT:600〜680?ƒ)

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号