The present invention relates to a manufacturing method of a transfer paper for co-fire for cell configuration of solid oxide fuel cell, and a transfer paper for co-fire for cell configuration of solid oxide fuel cell manufactured thereby. The purpose of the present invention is to reduce cost of product through energy reduction followed by shortening processing time by completing an SOFC cell only with an electrode coating process and a hardening process. The manufacturing method of the transfer paper for co-fire for cell configuration of solid oxide fuel cell comprises the steps of: manufacturing a first transfer paper for co-fire by transferring anode paste to a transfer paper through an SUS mask having 65-75 ��of emulsion film and 300-350 mesh of wire diameter, and transferring anode functional layer paste and electrolyte paste successively on the top surface of the transferred anode paste layer, then drying the result naturally at 20-40; and manufacturing a second transfer paper for co-fire by screen-transferring interconnect paste on a transfer paper through an SUS mask having 65-75 ��of emulsion film and 300-350 mesh of wire diameter, and transferring cathode functional layer and cathode paste successively on the top surface of the transferred interconnect paste, then drying the result naturally at 20-40. [Reference numerals] (AA) Anode to Electrolyte co-fire transfer paper;(BB) Interconnect to Cathode co-fire transfer paper
机译:本发明涉及一种用于固体氧化物燃料电池的单元构造的共烧转印纸的制造方法,以及由此制造的用于固体氧化物燃料电池的单元构造的共烧转印纸的制造方法。本发明的目的是通过仅通过电极涂覆工艺和硬化工艺完成SOFC电池来通过降低能量,随后缩短加工时间来降低产品成本。固体氧化物燃料电池的电池共烧转印纸的制造方法包括以下步骤:通过将阳极浆料通过具有65-75的SUS掩模转印到转印纸上来制造用于共烧的第一转印纸。乳化膜和线径300-350目,并依次在转移的阳极糊剂层的顶面上转移阳极功能层糊剂和电解质糊剂,然后将结果自然干燥20-40;并通过将具有65-75英寸乳化膜和300-350目线径的SUS掩模在转移纸上丝网转移互连浆料,并转移阴极功能层和阴极浆料,从而制造用于共烧的第二转移纸依次在转移的互连膏的顶面上,然后将结果自然干燥至20-40。 [附图标记](AA)阳极至电解质共烧纸;(BB)互连至阴极共烧纸

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号