formula aMO bM'(SSe1- ) cAl2O3 dB2O3 eP2O5:xEu yLn I provide a long-afterglow luminescent material is represented , and where M is Sr, Ca, and one or more elements selected from Ba, and Mg, M ' is at least one element selected from Sr, Ca, and Ba, Ln is Nd, Dy, Ho, Tm, La, Ce, Er, Pr, and at least one element selected from Bi and Sm, a, b, c, d, e, x, y are each a number of moles , 0.5 & a & 6.0, 0.0001 b 2.0, 0.5 c 9.0, 0 d 1.0, 0 e 1.0, 0.00001 x 0.25, 0.00001 y 0.3, 0 1.0 , where 0.5 & (a + b) 6.0, 0 & a (d + e) 1.0. The production process is a high temperature solid phase reaction comprising the reduction step following the oxidation step .
展开▼
机译:公式aMO bM'(SSe 1 Sub> - Sub>)cAl 2 Sub> O 3 Sub> dB 2 Sub> O 3 Sub> eP 2 Sub> O 5 Sub>:xEu yLn我提供了一种长余辉发光材料,其中M是Sr,Ca和选自Ba和Mg,M'的一种或多种元素是选自Sr,Ca和Ba的至少一种元素,Ln是Nd,Dy,Ho,Tm,La,Ce,Er,Pr和至少一种元素选自Bi和Sm的a,b,c,d,e,x,y分别为多个摩尔数,0.5≤n。 & 6.0、0.0001 b 2.0、0.5 c 9.0、0 d 1.0、0 e 1.0、0.00001 x 0.25、0.00001 y 0.3、0 1.0,其中0.5& (a + b)6.0,0& (d + e)1.0。生产过程是高温固相反应,其包括在氧化步骤之后的还原步骤。
展开▼